Hastelloy C276 Sintered Filters

For the duties 316L walks away from: HCl, wet chlorine, hypochlorite, mixed acid service

Hastelloy C276 sintered filter cartridges

Overview

Before asking the price, place the duty. C276 runs 4-8× the price of 316L; the wrong direction is not an overspend, it is spending at all.

C276 is required when: hydrochloric acid (any concentration, ambient), wet chlorine gas or chlorine water (dry chlorine is the exception - 316L handles it), hypochlorite solutions (bleach, sodium hypochlorite), mixed acids (nitric + hydrochloric, sulfuric + hydrochloric), chlorinated organic media. The common thread: chloride ions with water present.

316L is enough when: neutral salt solutions at moderate concentration and temperature, dilute sulfuric (<5%), phosphoric and acetic acid, short-term flushed seawater exposure, sanitary food/pharma media.

Neither works when: concentrated nitric or fuming sulfuric (strong oxidizing - molybdenum actually hurts here), hot fluoride media (HF at any concentration needs case review), molten alkali metals. We will decline those orders rather than sell a failure.

One-line rule: chloride ions and water together, above 60 °C or below pH 4 → C276. Chloride without water (dry chlorine) → 316L. Fluoride present → neither; call us.

Specifications

GradeC276 (UNS N10276): Ni bal., Mo 15-17%, Cr 14.5-16.5%, W 3-4.5%, Fe 4-7%
Diameterφ20 - 200 mm
LengthUp to 1500 mm, to drawing
Rating0.2 - 100 μm
Continuous temperature≤600 °C (reducing; oxidizing discussed separately)
FittingsThread, flange, Tri-Clamp, 222/226, plain weld end
DocumentsMaterial certificate + spectrometric analysis per batch

FAQ

Wet vs dry chlorine - why does it matter?
Wet chlorine attacks 316L aggressively while dry chlorine is comparatively benign - water is the trigger, which is why C276 is specified for wet service.
Plate versions available?
Yes - C276 sintered plates share the same powder and furnace line.
Can we verify the alloy?
Spectrometric (PMI) analysis report ships with the batch; third-party re-test welcome.
Get a quote with a real answer in 30 minutes
Send your medium, temperature, pressure and target rating to [email protected] - drawings and annual quantities welcome. Free samples; material certificate and measured bubble-point / permeability data with every batch. Lead time 7-15 days standard, 10-20 for composite builds.
Email [email protected]

Related

316L CartridgesAll CartridgesDual-Material Composite